I've almost exclusively used WEST till this build and I know what it can do. I've never used 207 hardener, only their 206, slow, hardener sometimes with less than stellar results (as compared to the deck and cockpit of your MC 16.5).Heard of MAS, EAST, System 3. CLC seams to like MAS so I'm giving it a try. Do you take weather (even if inside) into account when you want a good clear finish with 105/207? Your bright finish deck et'c makes me rethink my choice of resins, at least on the bright finshed areas.