I'd go with the 4 oz on the deck and roll on a couple of fill coats as soon as you can. That's when the epoxy is still a bit tacky but not so tacky it pulls foam pieces off your roller. I've switched to fast hardener for laminating and fill coats so I can get three coats of epoxy on in a day. Adds some excitement to the project trying to beat the pot life! Even with slow hardener you'll get the first fill coat on the same day. Christmas won't be a problem timewise.
George K
In Response to: deck glass by Jay on Dec 10, 2006
Replies:
- Re: deck glass by Derik s on Dec 11, 2006
-
Re: deck glass by Ed, NY on Dec 11, 2006
- Re: deck glass by Laszlo on Dec 12, 2006
-
Re: deck glass by Mac on Dec 12, 2006
- Rub Strips/Rails by Mac on Dec 12, 2006
- everything is optional by LeeG on Dec 12, 2006
-