Builders' Forum Archives |
Re: 207 hardenener
Posted by Brad Shook on Nov 1, 2005
Chris,
I've been bldg. 3 CH17 LT's this fall and I bought some 105 Resin and 206 West System to use for filleting and bonding. I used it for coating/filleting/tapeing one of the boats hatches and it DID indeed blush a little, but it's not "yellow" when cured by any means. I would use it for the interior, but maybe not for the exterior as it is a little "amber" colored when cured. ...bon chance, Brad
In Response to: 207 hardenener by Chris on Nov 1, 2005
Replies:
- Re: 207 hardenener by Chris on Nov 1, 2005
- Re: 207 hardenener by craig on Nov 1, 2005
- OUI! by Brad Shook on Nov 1, 2005
-
Re: 207 hardenener by Brad Shook on Nov 2, 2005
- Re: 207 hardenener by Chris on Nov 2, 2005
- Re: 105/207 hardenener by Brad Shook on Nov 2, 2005
- Re: 105/207 hardenener by Chris on Nov 2, 2005
- Re: 105/207 hardenener by Brad Shook on Nov 2, 2005
- Re: 207 hardenener by Chris on Nov 2, 2005